Dual-Axis Electromechanical Creep Testing Machine With Furnace
Manufactured by 3R Industries
Offering two independent tests in a single furnace, this dual-axis electromechanical creep test machine gives you double productivity for half the budget.
It’s ideal for labs carrying out high-temperature creep tests who want to increase their throughput, cut their costs, optimise space, or modernise their testing equipment.
The intuitive control interface and advanced connectivity provide a smooth operator experience (no moving masses), while ensuring the precision and thermal stability essential for materials research and quality control labs.
Price on quotation
Benefits
- Reproduces complex thermal and mechanical conditions to validate the behaviour of materials subjected to extreme environments up to 1200 °C.
- Combines precision electromechanical technology with an innovative dual-axis architecture.
- Perform two complete tests in parallel, without interference.
- Compact, robust and easy to use.
- Integrates seamlessly into any laboratory environment.
- Reduce your investment and operating costs by 50%.
- Compliant with creep testing standards ASTM E139-11 and ISO 204 for reliable results.
- Install up to 4 m machines per square metre, without modifying your laboratory environment.
- Remote supervision, automatic alerts and integrated remote maintenance for continuous and secure monitoring.
- Optimised electromechanical design reduces your energy consumption and controls your environmental footprint.
Industry Types: Energy & Environment, Research & Education.
| Dimensions (L x W x H) | 600 x 935 x 2120 mm |
| Capacity | 25 kN per axis |
| Stroke | 160 mm |
| Displacement Resolution | 2 nm |
| Max. speed under load | 1,4 mm/s |
| Temperature range | 20°C – 1200°C |
| Thermal stability | ±3°C |
| Power supply | 230 V – 20 A – 4,6 kW |
| Weight | 450 kg |